    A rubber part comes out of the mold with blisters on the surface, voids inside, or a texture that looks like a sponge.

     

    This is one of the most common defects in rubber molding. And it almost always comes down to the same thing: gas that couldn't escape.

     

    Where does the gas come from? Three places.

     

    The Cure Wasn't Right

    Cure temperature too low, or time too short. The volatiles produced during vulcanization never got a chance to escape. They stay trapped inside. Fix: find out why the cure was incomplete, then adjust temperature or time.

     

    Cure temperature too high. The surface cures too early, forming a skin that blocks air, water vapor, and volatiles from escaping. Thick parts are especially vulnerable. Fix: lower the temperature.

     

    Compound cures too fast. Internal volatiles don't have time to escape before the rubber hardens. Fix: adjust the formula to extend the induction period.

     

    The Gas Had Nowhere to Go

    Cure pressure too low. Gas and volatiles sitting in the cavity can't get out. Fix: increase pressure.

     

    Pressure applied too fast. The mold closes quickly, and gas doesn't have time to escape. Fix: close the mold slowly, and let pressure build gradually.

     

    No venting, or venting at the wrong time. Most rubber parts need venting. Too early or too late causes other problems. Fix: get the vent timing right.

     

    Poor mold structure. For complex parts, gas gets trapped in dead corners. Fix: use a multi-insert mold so gas escapes through the seams. Add vent grooves where voids tend to appear. Don't make the cavity too deep.

     

    Improper loading. For molds with complex geometry or dead corners, the compound needs to be distributed evenly. Otherwise, air gets trapped. Fix: distribute the compound evenly across the cavity.

     

    The Compound Brought Gas In

    Air or moisture trapped in the compound. Usually from poor mixing or improper storage. Fix: improve mixing quality. Keep mixed compound sealed or dried.

     

    Not enough material loaded. Besides causing short shots, it leaves the interior less dense — which shows up as voids. Fix: load the correct amount.

     

    The common thread: gas needs a way out. Whether it's the cure, the venting, or the compound itself — if gas can't escape, it stays in the part.


    References
    #ADVANCED MANUFACTURING
    Discover Other Injection Moulding News
    #SPECIAL
    Plastics Products Everywhere
    08-08
    Have you ever thought about how much plastic is utilized in commonplace goods? If you immediately glance around you, you will see that hundreds of products you used in the previous day were made of pl...
    Ways to Express the Formula of Viscoelastic Damping Materials
    08-14
    There are four ways to present the formula of viscoelastic damping materials, usually in the form of a proportion table.(1) Basic formula form. It's expressed with the main polymer in the formula ...