Injection Molded Parts Out of Spec? Usually These 5 Causes

Table of Content [Hide]

    You‘ve approved the mold. You’ve dialed in the process. The first batch of injection molded parts comes out within spec.

     

    Then the next batch is different. Same machine, same settings, same material — but the dimensions won‘t stay put.

     

    This is one of the most common complaints in injection molding. And it’s not one problem — it‘s several. Here’s what causes it and how to fix it.

     

    What Causes Dimensional Instability

    Material. Semi-crystalline resins shrink more and have a wider shrinkage range than amorphous resins. Switching material batches can change shrinkage, even with the same resin grade. Irregular pellet size causes uneven feeding.

     

    Process. Barrel or nozzle temperature too high — the part doesn‘t cool enough. Injection pressure too low, fill time too short — the cavity isn’t completely filled. Holding pressure too low, holding time too short — not enough compensation for shrinkage. Mold temperature uneven — different sections shrink at different rates.

     

    Mold design. Runner and gate dimensions inconsistent — uneven filling. Insufficient mold rigidity — the mold deforms under cavity pressure, and part dimensions change with it.

     

    Machine. Unstable feeding, back pressure, temperature control, or screw speed. Worn ejector pins deform parts during ejection.

     

    Measurement. Different methods, timing, or temperature — the same part measures differently. Parts need about 24 hours to stabilize after ejection. Measuring too early gives inconsistent results.

     

    How to Fix It

    Material control. Uniform pellet size. Thorough drying. Strict control of regrind ratio. The resin‘s shrinkage range must not exceed your part tolerance.

     

    Process control. Lock down the process window. If parts are oversized: lower melt temperature and injection pressure, reduce injection and holding time, increase mold temperature, shorten cooling. If undersized: do the opposite.

     

    Mold design. Balance gate and runner layout. For tight-tolerance parts, limit cavities to 1–2, maximum 4. Use high-rigidity mold steel. Use corrosion-resistant steel for corrosive plastics, wear-resistant steel for glass-filled materials.

     

    Machine maintenance. Check feeding, heating, hydraulic, temperature control, and voltage stability.

     

    Measurement standard. Use the standard method and temperature. Measure only after the part is fully cooled and stabilized — about 24 hours after ejection.

     

    The First Step

    Don‘t start by adjusting the process. Start by identifying the source: material batch, process drift, mold rigidity, machine stability, or measurement method.

     

    We build molds and run production for tight-tolerance injection molded parts. If you have a drawing and a tolerance requirement, send it over. We’ll quote the tool and the parts.


    References
    #ADVANCED MANUFACTURING
    Discover Other Injection Moulding News
    #SPECIAL
    Structure of Thermoplastic Elastomers
    05-05
    Although the synthesis methods of various block copolymer - type TPEs are different, and their specific structures and properties may also vary, they share the most important commonalities. That is, t...
    Demolding in Injection Molding: A Guide to Proper Techniques
    03-23
    Demolding is the final step in the injection molding cycle. Improper demolding can cause uneven force distribution and deformation of the product during ejection, leading to defects. Two Main Demoldin...