    POM is used in fuel systems, powertrains, and a long list of other automotive parts. These aren‘t easy places for any plastic to survive. So what makes POM the go-to?

    7-things-you-should-know-before-injection-molding-pom1.jpg

     

    What Is POM?

    POM — polyoxymethylene, or acetal — is a semi-crystalline engineering thermoplastic.

     

    It comes in two types:

    • Homopolymer: better creep resistance, 10–15% higher tensile strength, stiffer at high temperatures, better low-temperature impact.

    • Copolymer: better dimensional stability, slightly better chemical resistance, lower porosity in extrusion.

     

    What Automotive Parts See in POM

    Creep resistance. POM has one of the highest creep resistances among thermoplastics. Gears mesh, latches hold, fuel components sit under pressure — for years. Ordinary plastics slowly deform. POM doesn’t.

     

    Fatigue resistance. Door locks, window regulators, seat belt components. These cycle dozens of times a day. POM handles it without cracking.

     

    Low water absorption. This is where POM beats PA (nylon). PA absorbs moisture and changes dimensions. POM barely absorbs water. Summer heat, winter freezing, rain — dimensions stay stable.

     

    Chemical resistance. Gasoline, engine oil, grease, alcohol, solvents. Fuel system parts contact gasoline directly. Powertrain parts contact oil. POM handles both.

     

    Self-lubrication. Friction coefficient: 0.2 static, 0.35 dynamic. Gears, bearings, slides, cams run smoothly without added lubricant.

     

    Where It‘s Used

    • Fuel systems: pumps, fuel lines, power valves.

    • Powertrain: gears, bearings, cams.

    • Body and interior: door handles, lock assemblies, window regulators, seat belt components.

    • One part you touch every day: the seat belt buckle. That clicking latch? POM.

     

    But There Are Limits

    • No solvent welding. A side effect of its good solvent resistance.

    • Attacked by strong acids, bases, oxidizers. Avoid strong alkaline cleaners on fuel system parts.

    • UV sensitive. Outdoor exposure causes slow surface degradation. POM isn’t the first choice for long-term outdoor parts.

    • Not self-extinguishing. Long exposure at high temperatures can release formaldehyde. Process control matters.

     

    Injection Molding POM: What Matters

    • POM is heat-sensitive. It decomposes severely at 240°C.

    • At 210°C, residence time must not exceed 20 minutes.

    • At 190°C, keep it under 1 hour.

    • Use the lowest practical melt temperature and shortest residence time.

    • Melt viscosity is shear-sensitive. Don‘t try to improve flow by raising temperature. Increase injection rate and pressure instead.

    • Mold temperature: 80–100°C. Thin-wall or complex parts can run slightly hotter at the barrel — but never above 210°C.

    • Injection pressure has little effect on mechanical properties. It mainly affects flow and surface quality.

    • Thick-wall parts: slow injection. Thin-wall parts: fast injection.

    References
    #ADVANCED MANUFACTURING
    Discover Other Injection Moulding News
    #SPECIAL
    Troubleshooting Guide
    05-21
    Strict process control is the key to producing products that are completely consistent, meet strict tolerances, and satisfy various quality standards. The troubleshooting guide described here mainly a...