    When you're designing a plastic part, it's easy to focus on how it looks and how it works. But if you ignore how it will be molded, you're setting yourself up for defects, delays, and higher costs.

     

    Here are six common design mistakes that cause problems on the mold and in the part — and what to do instead.

     

    Ignoring Where the Parting Line Lands

    The parting line is where the two halves of the mold meet. Its location affects how the part looks.

     

    If it ends up on a visible surface, it can leave a mark that ruins the appearance. In some cases, you can hide it with a decorative line, like a groove or step (see Figure 1-1). Or you can design the top cover to be larger than the base so the line falls in a less obvious spot (see Figure 1-2).

     

    Fix: Place the parting line where it won't be seen, or design a feature that disguises it.


     

    Making the Gate Design Impossible

    The gate is where plastic enters the mold. If the part shape is too complex or the wall thickness varies too much, it becomes very hard to design a gate that fills properly and leaves an acceptable mark.

     

    Fix: Think about gate location early. Consider where the gate mark will be and whether it can be hidden or trimmed easily. Keep the part geometry friendly for mold filling.

     

    Using Sharp Corners and Thin Points

    Sharp corners create stress concentration — that's where cracks start. Thin, pointed sections are weak and break easily.

     

    Fix: Use generous radii. A good rule of thumb: inner corners should have a radius of at least half the wall thickness, and outer corners about 1.5 times the wall thickness. Minimum radius should be 0.5 mm. This also protects the mold itself — sharp core pins break.

     

    Designing Curved or Stepped Parting Lines

    If the parting line has curves or steps, the mold becomes much harder to make. That adds cost and lead time.

     

    Fix: Keep the parting line as simple and straight as possible. If curves are unavoidable, make sure they're gentle and easy to machine.

     

    Creating Asymmetrical Parts

    Asymmetry causes uneven shrinkage and warpage. It also makes the mold more complex and can lead to filling problems.

     

    Fix: Design your part as symmetrical as possible. For complex shapes, avoid walls that meet at very small angles. A wider angle means better flow and less stress.

     

    Forgetting About Sink Marks, Warpage, and Weld Lines

    These defects don't show up until you mold the part. But they start with design.

    • Sink marks happen when thick sections cool slower than thin ones.

    • Warpage comes from uneven cooling or fiber orientation.

    • Weld lines form where melt fronts meet, and they're weak points.

    • Cracks and local deformation often come from stress concentration or poor ejection.

     

    Fix: Keep wall thickness uniform. Use ribs instead of thick sections. Place gates so weld lines land in non-critical areas. And always think about how the part will cool and eject.

    References
    #ADVANCED MANUFACTURING
    Discover Other Injection Moulding News
    #SPECIAL
    Why Should Injection Molds Be Tested? What is the Purpose of Mold Testing?
    11-25
    (1) Reasons for Testing Injection MoldsMold testing is the process of actually injecting plastic into a mold designed and manufactured for plastic products on an appropriate injection molding machine....
    Nylon 6 (PA 6)
    12-03
    (1) Barrel TemperatureFeed Zone: 60–90°C (70°C)Zone 1: 230–240°C (240°C)Zone 2: 230–240°C (240°C)Zone 3: 240–250°C (250°C)Zone 4: 240–250°C (250°C)Zone 5: 240–250°C (250...